Krylon fusion peeling off?

My buddy and I both built internal glass overflows and painted them with krylon fusion paint. He water tested his and when he was draining it, the paint started peeling off the glass overflow... Any ideas why this would happen? The test was done with fresh water, Just curious I am wondering if it is the glass he used, or if KF doesn't bond well to glass when it becomes wet. I have a HOB overflow that acrylic painted with KF and have never had an issue with it.