View Single Post
  #35  
Old 01/09/2008, 07:04 PM
spazz spazz is offline
no time for spell check!
 
Join Date: Nov 2003
Location: coon rapids,mn
Posts: 2,209
Quote:
Originally posted by H20ENG
Jon,
I would test both acrylic to acrylic, and acrylic to glass.

I know when they set the 2.5" acrylic tunnels at my old job, they used a very wicked Sika primer to etch the acrylic first.

Now theres another name that I've used alot of - Sikaflex. Gooey, sticky, great stuff Being around boats, you probably have used it too.
yep this is exactly what i would do.. test acrylic to acrylic and acrylic to glass.
there is a primer they have for the dow corning 795 that you might want to look into. also the promer that H20ENG recomends would be good to try that way to get different primers with different strenghts. you cna find out which one is the best for that application.
__________________
a wise man once told me....
" there is no right way to build a reef tank but there is alot of wrong ways to build a reef tank".